+86 371 55057610

inquiry@xsteelplate.com

  • S275NL
  • S275NL

S275NL

  • Steel Standard: EN 10025-3
  • Rolling Type: Structural steel plate,low alloy steel plate
  • Thickness: 6mm-500mm
  • Width: 1500mm-4200mm
  • Length: 3000mm-18000mm
  • Heat Treatment: Normalised
(※ Click this button to inquiry)
■ Overview
Low temperature impacting test under -50 centigrade shall be done for structural steel plate S275NL.On longitudinal direction,the minimum values of impacting energy for S275NL test pieces shall be above 27 J,and on transverse direction,the minimum values of impacting energy for S275NL shall be above 16J according to steel standard EN 10025-3.Steel plate S275NL shall be supplied normalized or in an equivalent condition obtained by normalizing rolling.Xinsteel offer steel plate S275NL all over the world.
■ Full Data
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
 
■ Techicals

Mechnical property for S275NL Structural steel:

Thickness (mm)
S275NL ≤ 16 > 16 ≤ 40 > 40 ≤ 63 > 63 ≤ 80 > 80 ≤ 100 > 100 ≤ 150 > 150 ≤ 200 > 200
Yield strength (≥Mpa) 275 265 255 245 235 225 215 205
  ≤ 100 > 100 ≤ 200 > 200
Tensile strength (Mpa) 370-510 350-480 350-480

Chemical composition for S275NL Structural steel (Heat Analysis Max%)

Main chemical elements composition of S275NL
C Si Mn P S Nb V
0.16 0.40 0.50-1.50 0.025 0.020 0.05 0.05
Al(total) Ti Cr Ni Mo Cu N
≥0.02 0.05 0.30 0.30 0.10 0.55 0.015

Inquiry >>
Your name :
Your tel :
* Your mail :
Your company :
Your country :
* Inquiry :